Trusted Team

Local Professionals

Full-flake polyaspartic system · Back in use in 48 hours

Three-Car Garage Flake Floor in Vernon Hills, IL

A stained, cracked slab ground, repaired and coated with full flake. Walk-on the same evening, drive-on two days later.

GET A FREE QUOTE

Why We Built It This Way

Why not just a solid color coating?

A solid color coating would have covered this garage for less. We recommended the full flake broadcast instead because of what this particular floor has to deal with: three cars coming in wet from November through March. A flat coating goes slick the moment snowmelt sits on it, while aggregate broadcast to refusal keeps its traction with water on the surface — and hides the tire grit and scuffing a single-color floor shows within a season.

The polyaspartic topcoat was the second decision. It costs more than a standard epoxy clear, and it buys the homeowner two things: the garage comes back into use in hours instead of days, and the finish holds its color where afternoon sun reaches through the open door, which is where epoxy clears tend to yellow first.

Neither choice would matter without the first day. Most garage floors that peel were never properly ground — the coating sat on a sealed slab and let go in the first freeze. We charge for preparation on every job because it is the part that decides whether a floor lasts two winters or many years, and this one is covered by a written workmanship and material warranty because we know what went underneath it.

Two Days on Site, Hour by Hour

What happens between an empty garage and a finished floor

Day 1, 8:00 a.m. — Grinding. Two installers ran diamond tooling across all 720 square feet until the concrete pores were open, vacuuming behind the grinder so nothing settled back onto the surface. The crack in the third bay was chased out, filled with a rigid polyurea, and ground flush.

Day 1, 2:00 p.m. — Moisture test, then primer. The slab read within range, so the pigmented epoxy primer went down the same afternoon instead of costing the homeowner a day of waiting.

Day 2, 9:00 a.m. — Flake broadcast. Cabin Fever FB-127 in 1/8" went into the wet base coat until the floor stopped taking it. Broadcasting to refusal is what builds the texture into the floor rather than scattering it across the top.

Day 2, 1:00 p.m. — Scrape, sweep, topcoat. The loose flake came off and a polyaspartic topcoat sealed the rest into one continuous surface.

That evening the garage was walk-on. Two days later the cars came back in.